Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 12 % Show Supplier Material materials with Elongation of 12 % |
Tensile strength | 23.0 °C | 800 - 950 MPa Show Supplier Material materials with Tensile strength of 800 - 950 MPa |
Yield strength | 23.0 °C | 600 MPa Show Supplier Material materials with Yield strength of 600 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.12 - 0.22 % Show Supplier Material materials with Carbon of 0.12 - 0.22 % |
Chromium | 15 - 17 % Show Supplier Material materials with Chromium of 15 - 17 % |
Manganese | 1.5 % Show Supplier Material materials with Manganese of 1.5 % |
Nickel | 1.5 - 2.5 % Show Supplier Material materials with Nickel of 1.5 - 2.5 % |
Phosphorus | 0.04 % Show Supplier Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Supplier Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Supplier Material materials with Sulfur of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Precison components, General Engineering |