Kynar Superflex® 2501-20

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Superflex® resin is a thermoplastic fluorinated polymer.

The properties are the same as standard grades: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior.

More over, this grade is very flexible and is suitable in electrical isolation cable, tubing and co-extrusion.

This grade is available as powder form for injection, extrusion, compression

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.79 g/cm³

Show Supplier Material materials with Density of 1.79 g/cm³

dry

ISO 1183

Limiting oxygen index

44 %

Show Supplier Material materials with Limiting oxygen index of 44 %

dry

ISO 4589-1/-2

Water absorption

0.03 %

Show Supplier Material materials with Water absorption of 0.03 %

Sim. to ISO 62

Mechanical

PropertyValueConditionTesting StandardComment

Elastic modulus

0.35 GPa

Show Supplier Material materials with Elastic modulus of 0.35 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

min. | nominal

Elongation at yield

18 %

Show Supplier Material materials with Elongation at yield of 18 %

dry

ISO 527-1/-2

Yield strength

10 MPa

Show Supplier Material materials with Yield strength of 10 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureComment

Glass transition temperature

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

dry

ISO 11357-1/-2

10°C/min

Heat deflection temperature

31 °C

Show Supplier Material materials with Heat deflection temperature of 31 °C

dry

ISO 75-1/-2

2 MPa

Melting point

122 °C

Show Supplier Material materials with Melting point of 122 °C

dry

ISO 11357-1/-3

10°C/min

Flammability

At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 mm IEC 60695-11-10: V-0 and yellow card available

Electrical

PropertyValueConditionTesting Standard

Dielectric strength

12 kV/mm

Show Supplier Material materials with Dielectric strength of 12 kV/mm

dry

IEC 60243-1

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

5.8 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 5.8 cm³/10min

dry

ISO 1133

232°C/3.8kg

Technological properties

Property
Application areas

Fluoropolymer Processing Aids

Certifications

Yellow Card