5083 Al-FORMODAL® 024 elox

Alternative and trade names
FORMODAL® 024 elox
Want to keep this datasheet? Save it now in your required format

Description

Aluminium cast plate, The mechanical properties are investigated in O3 condition

Related Standards

Equivalent Materials

This material data has been provided by BIKA.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.66 g/cm³

Show Supplier Material materials with Density of 2.66 g/cm³

Dimension

PropertyValue

Thickness

5 - 500 mm

Show Supplier Material materials with Thickness of 5 - 500 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

70 GPa

Show Supplier Material materials with Elastic modulus of 70 GPa

Elongation

23.0 °C

15 %

Show Supplier Material materials with Elongation of 15 %

A10 mm

Hardness, HBW

23.0 °C

70 - 80 [-]

Show Supplier Material materials with Hardness, HBW of 70 - 80 [-]

Tensile strength

23.0 °C

230 - 290 MPa

Show Supplier Material materials with Tensile strength of 230 - 290 MPa

Yield strength

23.0 °C

110 - 130 MPa

Show Supplier Material materials with Yield strength of 110 - 130 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

2.35E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.35E-5 1/K

Mean values between 20°C and the mentioned temperature

Specific heat capacity

23.0 °C

900 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 900 J/(kg·K)

Thermal conductivity

23.0 °C

110 - 140 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 110 - 140 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

1.60E+7 - 1.80E+7 S/m

Show Supplier Material materials with Electrical conductivity of 1.60E+7 - 1.80E+7 S/m

Chemical properties

PropertyValueComment

Aluminium

Balance

Chromium

0.05 - 0.25 %

Show Supplier Material materials with Chromium of 0.05 - 0.25 %

Copper

0.1 %

Show Supplier Material materials with Copper of 0.1 %

Iron

0.4 %

Show Supplier Material materials with Iron of 0.4 %

Magnesium

4 - 4.9 %

Show Supplier Material materials with Magnesium of 4 - 4.9 %

Manganese

0.4 - 1 %

Show Supplier Material materials with Manganese of 0.4 - 1 %

Other

0.15 %

Show Supplier Material materials with Other of 0.15 %

Total

Silicon

0.4 %

Show Supplier Material materials with Silicon of 0.4 %

Titanium

0.15 %

Show Supplier Material materials with Titanium of 0.15 %

Zinc

0.25 %

Show Supplier Material materials with Zinc of 0.25 %

Technological properties

Property
Anodizing

very good

Application areas

Tool making, mould making and model making; Laser technology; Cover plates; Printing technology; Fixture construction; Electronics and optical industry; Packaging technology; Medical technology

Corrosion properties

very good

Dimensional stability

very good

General machinability

very good

Welding

WIG: good, MIG: good, Resistance welding: good