Barium zirconium yttrium ytterbium cerate (BZCYYb) Powder

Want to keep this datasheet? Save it now in your required format

Description

BZCYYb is supplied as fine, white submicron powder with a chemical purity > 99%.

This material data has been provided by Cerpotech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Specific surface area

7 - 15 m²/g

Show Supplier Material materials with Specific surface area of 7 - 15 m²/g

Technological properties

Property
Application areas

solid oxide fuel cell, SOFC, solid oxide electolyzer cell, SOEC, membranes for hydrogen separation, protonic conductor, tubular ceramic fuel cell, composite electrode, cathode, electrolyte, catalyst

Chemical composition

BaZr0.7Ce0.1Y0.1Yb0.1O3, BaZr0.4Ce0.4Y0.1Yb0.1O3

Color

Fine, white powder

Processing history

Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices.