Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 10 - 13 % Show Material materials with Elongation of 10 - 13 % |
Hardness, Brinell | 23.0 °C | 200 - 220 [-] Show Material materials with Hardness, Brinell of 200 - 220 [-] |
Tensile strength | 23.0 °C | 700 - 760 MPa Show Material materials with Tensile strength of 700 - 760 MPa |
Yield strength | 23.0 °C | 400 - 500 MPa Show Material materials with Yield strength of 400 - 500 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 9.7 % Show Material materials with Aluminium of 9.7 % |
Copper | Balance |
Iron | 3.8 % Show Material materials with Iron of 3.8 % |
Lead | 1.75 % Show Material materials with Lead of 1.75 % |
Manganese | 1.3 % Show Material materials with Manganese of 1.3 % |
Nickel | 5 % Show Material materials with Nickel of 5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware, fasteners and fittings;General: Fasteners, gears, non-sparking safety tooling, thrust washers, valve guides, fluid handling equipment, valve spindles and components, bearings pins and bushes, thermostatic valves and worm wheels | |
Corrosion properties | Excellent general corrosion resistance | |
General machinability | Excellent machinability |