COLSPEED 90 is derived using the basis of a 10/5/5 aluminium bronze with an addition of finely dispersed lead particles with very good self-lubricating and anti-friction properties that improve performance in wear applications. It shows the following features and properties:
Element
Weight %
Comment
-
Balance
9.7 %
5 %
3.8 %
1.75 %
Application areas
Offshore & marine: Marine hardware, fasteners and fittings;General: Fasteners, gears, non-sparking safety tooling, thrust washers, valve guides, fluid handling equipment, valve spindles and components, bearings pins and bushes, thermostatic valves and worm wheels
Corrosion properties
Excellent general corrosion resistance
General machinability
Excellent machinability