Copper Nickel 90/10 Copper Alloy

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A

27 % at 20 °C

Hardness, Brinell HB

70 - 120 [-] at 20 °C

Tensile strength Rm

280 MPa at 20 °C

Yield strength YS

105 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

-

REM

Ni

10.5 %

Fe

1.5 %

Mn

0.75 %

This material data has been provided by Columbia Metals.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.