The material: 'BS NS104 Nickel Silver' you were looking for has been superseded by the one below.

BS NS104 Nickel Silver

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

NS104 (CuNi12Zn24) is the standard grade of nickel silver for general purpose applications. Primarily a sheet grade, NS 104 contains 12% nickel and is utilised where the additional strength of half hard temper material imparts rigidity and spring properties. The presence of nickel provides corrosion and tarnish resistance to levels well in excess of normal brasses. Material of this temper is still cold workable and readily fabricated by bending, punching, stamping etc. NS104 is soldered and silver brazed without difficulty and is widely used for electrical and electronic components as well as for general engineering and aesthetic purposes.

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.65 g/cm³

Show Material materials with Density of 8.65 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

123 GPa

Show Material materials with Elastic modulus of 123 GPa

Elongation

23.0 °C

30 %

Show Material materials with Elongation of 30 %

Hardness, Vickers

23.0 °C

140 [-]

Show Material materials with Hardness, Vickers of 140 [-]

Tensile strength

23.0 °C

530 MPa

Show Material materials with Tensile strength of 530 MPa

Yield strength Rp0.2

23.0 °C

320 MPa

Show Material materials with Yield strength Rp0.2 of 320 MPa

Thermal

PropertyTemperatureValue

Melting point

1000 - 1060 °C

Show Material materials with Melting point of 1000 - 1060 °C

Thermal conductivity

23.0 °C

33 W/(m·K)

Show Material materials with Thermal conductivity of 33 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

4.64E+6 S/m

Show Material materials with Electrical conductivity of 4.64E+6 S/m

Electrical resistivity

23.0 °C

2.2E-7 Ω·m

Show Material materials with Electrical resistivity of 2.2E-7 Ω·m

Specific Electrical conductivity

8 % IACS

Show Material materials with Specific Electrical conductivity of 8 % IACS

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1.05 [-]

Show Material materials with Relative magnetic permeability of 1.05 [-]

max.

Chemical properties

PropertyValueComment

Copper

60 - 65 %

Show Material materials with Copper of 60 - 65 %

Iron

0.25 %

Show Material materials with Iron of 0.25 %

max.

Lead

0.04 %

Show Material materials with Lead of 0.04 %

max.

Manganese

0.05 - 0.3 %

Show Material materials with Manganese of 0.05 - 0.3 %

Nickel

11 - 13 %

Show Material materials with Nickel of 11 - 13 %

Zinc

Balance

Technological properties

Property
Application areas

General: Architectural metalwork, panels and trim, holloware, musical instruments, medals and medallions, costume jewellery, nameplates, cosmetic cases, lamp caps, lighting fittings, platters, bowls, dials, relay and contact springs, medical, industrial and scientific instrument components

Cold Forming

Good cold working characteristics

Corrosion properties

Good corrosion resistance