General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10.28 g/cm³ Show Material materials with Density of 10.28 g/cm³ |
Dimension
Property | Value |
---|---|
Length | 1828 mm Show Material materials with Length of 1828 mm |
Width | 1.6 - 50.8 mm Show Material materials with Width of 1.6 - 50.8 mm |
Dimensions | Available widths: 1.6mm, 1.8mm, 3.2mm, 4.8mm, 6.4mm, 7.6mm, 7.9mm, 9.5mm, 12.7mm, 15.9mm, 19.1mm, 25.4mm, 31.8mm, 38.1mm, 44.5mm, 50.8mm |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 320 GPa Show Material materials with Elastic modulus of 320 GPa | |
Elongation | 23.0 °C | 12 % Show Material materials with Elongation of 12 % | in 1 in. |
Hardness, Vickers | 23.0 °C | 220 [-] Show Material materials with Hardness, Vickers of 220 [-] | |
Tensile strength | 20.0 °C | 1035 MPa Show Material materials with Tensile strength of 1035 MPa | |
500.0 °C | 515 MPa Show Material materials with Tensile strength of 515 MPa | ||
1000.0 °C | 175 MPa Show Material materials with Tensile strength of 175 MPa | ||
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.8E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.8E-6 1/K |
Crystallization temperature | 1100 °C Show Material materials with Crystallization temperature of 1100 °C | |
Melting point | 2623 °C Show Material materials with Melting point of 2623 °C | |
Specific heat capacity | 23.0 °C | 259 J/(kg·K) Show Material materials with Specific heat capacity of 259 J/(kg·K) |
Thermal conductivity | 23.0 °C | 142 W/(m·K) Show Material materials with Thermal conductivity of 142 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 200.0 °C | 5.34E-8 Ω·m Show Material materials with Electrical resistivity of 5.34E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Molybdenum | 99.97 % Show Material materials with Molybdenum of 99.97 % | min |
Technological properties
Property | ||
---|---|---|
Application areas | In the missile industry Molybdenum is used for nose cones, high temperature structural parts, nozzles, leading edges of control surfaces, support vanes, re-entry cones, and heat radiation shields. In electronics Molybdenum is used for cathodes, magnetron end hats, x-ray tube components, filaments, and glass-to-metal seals. In high-temperature applications Molybdenum is used for: furnace windings, structural furnace members, and containers for components exposed to high temperatures. |