This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.

Near me

Customize your search with filters

Material Supplied by

Ed Fagan Inc.

Molybdenum Sheet Deep Draw Quality 3.2 mm

.XLSX
.PDF
Save

Description

Molybdenum is a refractory metal that is very useful in many industrial processes and applications that would not be possible with many of the more common metals and alloys. Refractory metals and alloys are extraordinarily resistant to heat and have unique physical properties.

Primary standard name

Equivalent standard names

Properties

Dimension

Thickness t

3.2 mm

Electrical

Electrical resistivity ρel

5.34E-8 Ω·m at 200 °C

General

Density ρ

10.28 g/cm³ at 20 °C

Mechanical

Elastic modulus E

329 GPa at 20 °C

Elongation A

12 % at 20 °C

in 1 in.

Hardness, Vickers HV

230 [-] at 20 °C

Tensile strength Rm

1035 MPa at 20 °C

Show chart

Thermal

Coefficient of thermal expansion α

4.8E-6 1/K at 20 °C

Crystallization temperature Tx

1100 °C

Melting point Tm

2623 °C

Specific heat capacity cp

259 J/(kg·K) at 20 °C

Thermal conductivity λ

138 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Mo

99.95 %

min

Technological properties

Application areas

Common applications of molybdenum are: cathodes, magnetron end hats, X-ray tube components, furnace windings, heat radiation shields

This material data has been provided by Ed Fagan Inc..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.