General
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Density | 25 °C | 1.02 g/cm³ Show Supplier Material materials with Density of 1.02 g/cm³ | ISO 1183-1 |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 1.9 GPa Show Supplier Material materials with Elastic modulus of 1.9 GPa | ISO 527-1/2 | 1 mm/min | |
Elongation | 15 % Show Supplier Material materials with Elongation of 15 % | ISO 527-1/2 | min. | 50 mm/min | |
Flexural modulus | 1.9 GPa Show Supplier Material materials with Flexural modulus of 1.9 GPa | ISO 178 | 2 mm/min | |
Flexural strength | 66 MPa Show Supplier Material materials with Flexural strength of 66 MPa | ISO 178 | 2 mm/min | |
Hardness, Ball Indentation | 81 MPa Show Supplier Material materials with Hardness, Ball Indentation of 81 MPa | ISO 2039-1 | ||
Impact strength, Charpy notched | -30 °C | 21 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 21 kJ/m² | ISO 179-1eA | |
23 °C | 31 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 31 kJ/m² | ISO 179-1eA | ||
Impact strength, Izod notched | -30 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 20 kJ/m² | ISO 180-1A | |
23 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 25 kJ/m² | ISO 180-1A | ||
Yield strength | 38 MPa Show Supplier Material materials with Yield strength of 38 MPa | ISO 527-1/2 | 50 mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 0.0001 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.0001 1/K | ISO 11359-1/2 | 23 to 55°C | ||
Vicat softening temperature | 95 °C Show Supplier Material materials with Vicat softening temperature of 95 °C | ISO 306 | 50 N | 50°C/h | ||
97 °C Show Supplier Material materials with Vicat softening temperature of 97 °C | ISO 306 | 50 N | 120°C/h | |||
Flammability | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (2mm): < 40 mm/min according to ISO 3795 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt volume-flow rate | 14 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 14 cm³/10min | ISO 1133 | 220°C/10Kg |
Shrinkage | 0.6 - 0.7 % Show Supplier Material materials with Shrinkage of 0.6 - 0.7 % | ISO 294-4 | 60x60x2 mm |
0.6 - 0.7 % Show Supplier Material materials with Shrinkage of 0.6 - 0.7 % | ISO 294-4 | 60x60x2 mm, Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Color | White to slightly yellowish. | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |