Alternative and trade names
Super-elastic nickel-titanium alloy
Want to keep this datasheet? Save it now in your required format

Description

Super-elastic nickel-titanium alloy

This material data has been provided by EPoS.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

6.5 g/cm³

Show Supplier Material materials with Density of 6.5 g/cm³

Mechanical

PropertyValueComment

Elongation

2.8 %

Show Supplier Material materials with Elongation of 2.8 %

Hardness, Vickers

280 - 320 [-]

Show Supplier Material materials with Hardness, Vickers of 280 - 320 [-]

HV 0.5

Max allowed stress

370 MPa

Show Supplier Material materials with Max allowed stress of 370 MPa

450 MPa

Show Supplier Material materials with Max allowed stress of 450 MPa

Technological properties

Property
Application areas

Mechanical, Aerospace, Biomedical

Other

Diameter 10 mm by 2-7 mm disks.

Diameter 15 mm by 2-7 mm disks.

20 x 10 x 2 to 8 mm heigh.

Special shapes upon request.

Processing methods

E-Forged™ from powders