WC-Ag

Want to keep this datasheet? Save it now in your required format

Description

WC reinforced Sterling Silver

This material data has been provided by EPoS.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

10.1 g/cm³

Show Supplier Material materials with Density of 10.1 g/cm³

Porosity

3 %

Show Supplier Material materials with Porosity of 3 %

Mechanical

PropertyValueComment

Hardness, Vickers

187 - 189 [-]

Show Supplier Material materials with Hardness, Vickers of 187 - 189 [-]

HV 0.2

Electrical

PropertyValue

Electrical resistivity

4.01e-08 Ω·m

Show Supplier Material materials with Electrical resistivity of 4.01e-08 Ω·m

Technological properties

Property
Application areas

Electrical contacts

Other

Diameter 10 mm by 2-10 mm disks.

Diameter 15 mm by 2-10 mm disks.

20 x 10 x 2 to 6 mm heigh.

Special shapes upon request.

Processing methods

E-Forged™ from powders