EN CuZn35Pb1 Leaded Brass

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Chemical properties

Element

Weight %

Comment

Zn

-

REM

Cu

62.5 - 64 %

Pb

0.8 - 1.6 %

Ni

0.3 %

Fe

0.1 %

More