Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % |
Arsenic | 0.02 - 0.15 % Show Supplier Material materials with Arsenic of 0.02 - 0.15 % |
Copper | 61 - 63 % Show Supplier Material materials with Copper of 61 - 63 % |
Iron | 0.1 % Show Supplier Material materials with Iron of 0.1 % |
Lead | 1.7 - 2.8 % Show Supplier Material materials with Lead of 1.7 - 2.8 % |
Nickel | 0.3 % Show Supplier Material materials with Nickel of 0.3 % |
Tin | 0.1 % Show Supplier Material materials with Tin of 0.1 % |
Zinc | Balance, REM |