Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Find Materials
Categories
EN CuZn38As DZR Brass
This material data has been provided by Fitco.
All categories
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % |
Arsenic | 0.02 - 0.15 % Show Supplier Material materials with Arsenic of 0.02 - 0.15 % |
Copper | 61.5 - 63.5 % Show Supplier Material materials with Copper of 61.5 - 63.5 % |
Lead | 0.2 % Show Supplier Material materials with Lead of 0.2 % |
Nickel | 0.3 % Show Supplier Material materials with Nickel of 0.3 % |
Tin | 0.1 % Show Supplier Material materials with Tin of 0.1 % |
Zinc | Balance, REM |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.