Chemical properties
Property | Value |
---|---|
Aluminium | 4 - 5 % Show Supplier Material materials with Aluminium of 4 - 5 % |
Copper | 65 - 68 % Show Supplier Material materials with Copper of 65 - 68 % |
Iron | 0.5 - 3 % Show Supplier Material materials with Iron of 0.5 - 3 % |
Lead | 0.2 - 0.8 % Show Supplier Material materials with Lead of 0.2 - 0.8 % |
Manganese | 0.5 - 3 % Show Supplier Material materials with Manganese of 0.5 - 3 % |
Nickel | 1 % Show Supplier Material materials with Nickel of 1 % |
Tin | 0.2 % Show Supplier Material materials with Tin of 0.2 % |
Zinc | Balance, REM |