SiC SIKA DENSITEC 13 H

Alternative and trade names
SIKA DENSITEC 13 H
Want to keep this datasheet? Save it now in your required format

Description

DENSITEC 13H granules are spray dried granules, bases on our standard black SINTEX 13C. The premix is doped with sintering additives, low content of temporary binder and pressing aids and is ready to be pressed. DENSITEC 13H is suitable for dry pressing, uniaxial and isostatic.

This material data has been provided by Fiven GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Bulk density

23.0 °C

0.88 g/cm³

Show Supplier Material materials with Bulk density of 0.88 g/cm³

Density

23.0 °C

3.19 g/cm³

Show Supplier Material materials with Density of 3.19 g/cm³

Particle size range

100 µm

Show Supplier Material materials with Particle size range of 100 µm

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

25 GPa

Show Supplier Material materials with Elastic modulus of 25 GPa

Flexural strength

23.0 °C

550 MPa

Show Supplier Material materials with Flexural strength of 550 MPa

Plane-Strain Fracture Toughnes

23.0 °C

3.5 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.5 MPa·√m

Rheological Properties

PropertyTemperatureValue

Hall flow

23.0 °C

30 s/50g

Show Supplier Material materials with Hall flow of 30 s/50g

Technological properties

Property
Application areas

Silicon Carbide Ready-To-Press granules for solid-state (SSiC) hot-pressed technical ceramics.

Chemical composition

Sinter additives: Carbon black, Boron Carbide; Binder: ~2%; Moisture Content: 0,6%; SiC type balance: SINTEX 13 C