SiC SIKA DENSITEC L

Alternative and trade names
SIKA DENSITEC L
Want to keep this datasheet? Save it now in your required format

Description

DENSITEC-L is used for production of liquid phase sintered SiC and is a spray granulated powder based on our standard black SINTEX 13C. The powder is doped with oxides, temporary binders and pressing aids, and is ready to be pressed into a green body.

Ashby charts

See where SiC SIKA DENSITEC L falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Bulk density

ρbulk

0.86 g/cm³ at 23 °C

Density

ρ

3.21 g/cm³ at 23 °C

Particle size range

drange

100 µm

Mechanical

Elastic modulus

E

24 GPa at 23 °C

Show Silicon Carbide materials with Elastic modulus of 24 GPa at 23 °C

Plane-Strain Fracture Toughnes

KIC

4.5 MPa·√m at 23 °C

Show Silicon Carbide materials with Plane-Strain Fracture Toughnes of 4.5 MPa·√m at 23 °C

Rheological Properties

Hall flow

HF

22.5 s/50g at 23 °C

Technological properties

Application areas

Silicon Carbide Ready-To-Press granules for solid-state (SSiC) sintered technical ceramics.

Chemical composition

SiC type: SINTEX 13C; Al2O3: 5,5%; Y2O3: 3,5%; Moisture content: 1%; Binder content (total organic): 6%

This material data has been provided by Fiven GmbH.