DENSITEC-L is used for production of liquid phase sintered SiC and is a spray granulated powder based on our standard black SINTEX 13C. The powder is doped with oxides, temporary binders and pressing aids, and is ready to be pressed into a green body.
See where SiC SIKA DENSITEC L falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Bulk density
ρbulk0.86 g/cm³ at 23 °C
Density
ρ3.21 g/cm³ at 23 °C
Particle size range
drange100 µm
Hall flow
HF22.5 s/50g at 23 °C
Application areas
Silicon Carbide Ready-To-Press granules for solid-state (SSiC) sintered technical ceramics.
Chemical composition
SiC type: SINTEX 13C; Al2O3: 5,5%; Y2O3: 3,5%; Moisture content: 1%; Binder content (total organic): 6%
This material data has been provided by Fiven GmbH.