Calcined Alumina (Fine/Super Ground) M-S1FG

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Precision Calcined Alumina is aluminum oxide that has been heated at temperatures in excess of 1,050°C (1,922°F) to drive off nearly all chemically combined water. In this form, alumina has great chemical purity, extreme hardness (9 on the Mohs hardness scale, on which diamond is 10), high density, and a high melting point (slightly above 2,000°C [3,632°F]).

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Bulk density

0.8 g/cm³

Show Supplier Material materials with Bulk density of 0.8 g/cm³

Loss on Ignition

0.3 %

Show Supplier Material materials with Loss on Ignition of 0.3 %

max.

Particle size range

4.0 - 7.0 µm

Show Supplier Material materials with Particle size range of 4.0 - 7.0 µm

Specific surface area

0.6000000000000001 - 1.5 m²/g

Show Supplier Material materials with Specific surface area of 0.6000000000000001 - 1.5 m²/g

BET

Thermal

PropertyValue

Melting point

2000.0 °C

Show Supplier Material materials with Melting point of 2000.0 °C

Chemical properties

PropertyValueComment

Aluminium

99.5 %

Show Supplier Material materials with Aluminium of 99.5 %

min. Al₂O₃

Iron

0.05

Show Supplier Material materials with Iron of 0.05

max. Fe₂O₃

Silicon

0.05

Show Supplier Material materials with Silicon of 0.05

max. SiO₂

Sodium

0.3

Show Supplier Material materials with Sodium of 0.3

max. Na₂O

Technological properties

Property
Application areas

GNPGraystar’s Calcined Alumina is used in refractory applications as well as ceramic applications including spark plugs, tap washers, pump seal, electronic substrates, grinding media, abrasion resistant tiles, cutting tools, bioceramics, body armor, laboratory ware, and wear parts for the textile and paper industries.


It is also used as a friction material in brake linings, in potting compounds to disperse heat, and in polishing, lapping, and buffing compounds.

Crystal structure

Alfa Alumina: 98%