Ytterbium Oxide 99.9%

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Ytterbium Oxide is a white to beige powder.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Loss on Ignition

1 %

Show Supplier Material materials with Loss on Ignition of 1 %

max. (1000°C/2 hrs)

Particle size D50

2.0 - 10.0 μm

Show Supplier Material materials with Particle size D50 of 2.0 - 10.0 μm

PSD

Chemical properties

PropertyValueComment

Calcium

0.015

Show Supplier Material materials with Calcium of 0.015

max. CaO

Cobalt

0.0005 %

Show Supplier Material materials with Cobalt of 0.0005 %

max. Co₃O₄

Iron

0.005

Show Supplier Material materials with Iron of 0.005

max. Fe₂O₃

Nickel

0.0005

Show Supplier Material materials with Nickel of 0.0005

max. NiO

Other

0.1

Show Supplier Material materials with Other of 0.1

Total Remaining RE-Oxides

Ytterbium

99.9 %

Show Supplier Material materials with Ytterbium of 99.9 %

min. Yb₂O₃

Technological properties

Property
Application areas

It is typically used as a phosphor activator and in coding material for security systems.