Description

GNPGraystar’s Fused High Monoclinic Zirconia Powder is produced by electro-fusion of zircon sand, in order to remove the silica, and exhibits superior thermal shock resistance.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValueComment

Aluminium

0.1

Show Supplier Material materials with Aluminium of 0.1

max. Al₂O₃

Iron

0.04

Show Supplier Material materials with Iron of 0.04

max. Fe₂O₃

Silicon

0.1

Show Supplier Material materials with Silicon of 0.1

max. SiO₂

Titanium

0.13

Show Supplier Material materials with Titanium of 0.13

max. TiO₂

Zirconium

99 %

Show Supplier Material materials with Zirconium of 99 %

min. ZrO₂

Technological properties

Property
Application areas

GNPGraystar’s Fused Monoclinic Zirconia Powder is excellent in metallurgical refractories such as zirconia nozzles and slide gates. It is also used in other refractories, ceramic pigments, auto brake additives, setting sands, and more.

Other

Particle size: Hollow Spheres or Customized