GNPGraystar’s Fused Yttria-Stabilized Zirconia is produced from special fusion of high purity zirconia with various amounts of yttrium oxide.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

6.1 g/cm³

Show Supplier Material materials with Density of 6.1 g/cm³

min.

Stabilization

85 %

Show Supplier Material materials with Stabilization of 85 %

min.

Chemical properties

PropertyValueComment

Aluminium

0.2

Show Supplier Material materials with Aluminium of 0.2

max. Al₂O₃

Calcium

0.2 %

Show Supplier Material materials with Calcium of 0.2 %

CaO

Iron

0.1

Show Supplier Material materials with Iron of 0.1

max. Fe₂O₃

Silicon

0.4

Show Supplier Material materials with Silicon of 0.4

max. SiO₂

Titanium

0.2

Show Supplier Material materials with Titanium of 0.2

max. TiO₂

Yttrium

8.8 - 9.8 %

Show Supplier Material materials with Yttrium of 8.8 - 9.8 %

Y₂O₃

Zirconium

88 %

Show Supplier Material materials with Zirconium of 88 %

ZrO₂

Technological properties

Property
Application areas

GNPGraystar’s Fused Yttria-Stabilized Zirconia is used for refractories, thermal spray coatings, plasma spraying, oxygen permeable membranes, ceramic rings, and many other applications.