Monoclinic Zirconia GNPR3

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Chemical Grade Monoclinic Zirconia is non-toxic and tasteless. It has good stability towards acid and alkaline solutions (excluding hot & thick H₂SO₄, HF, and H₃PO₄).

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size range

6.0 - 8.0 µm

Show Supplier Material materials with Particle size range of 6.0 - 8.0 µm

Specific surface area

10.0

Show Supplier Material materials with Specific surface area of 10.0

max.

Chemical properties

PropertyValueComment

Iron

0.005

Show Supplier Material materials with Iron of 0.005

max. Fe₂O₃

Silicon

0.02

Show Supplier Material materials with Silicon of 0.02

max. SiO₂

Sodium

0.003

Show Supplier Material materials with Sodium of 0.003

max. Na₂O

Titanium

0.005

Show Supplier Material materials with Titanium of 0.005

max. TiO₂

Zirconium

99.5 %

Show Supplier Material materials with Zirconium of 99.5 %

ZrO₂+HfO₂

Technological properties

Property
Application areas

GNPGraystar’s Chemical Grade Monoclinic Zirconia is used in precision ceramics, electrical components, glass additives, ceramic colored glazes, refractory materials, polishing applications, and synthetic jewelry

Color

White

Other

SSA & Particle Size can be customized