Sintered Magnesium-Aluminate Spinel SP90

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Fused MagnesiumAluminate Spinel is made of high purity raw materials in electric arc furnaces. The maximum amount of spinel crystals is achieved by using pure raw materials and electric arc furnaces. The product has a high thermal shock resistance and slag corrosion resistance, and good refractoriness.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

3.2 g/cm³

Show Supplier Material materials with Density of 3.2 g/cm³

Porosity

1.2 - 2.6 %

Show Supplier Material materials with Porosity of 1.2 - 2.6 %

Water absorption

1 %

Show Supplier Material materials with Water absorption of 1 %

max.

Chemical properties

PropertyValueComment

Aluminium

90 %

Show Supplier Material materials with Aluminium of 90 %

Al₂O₃

Calcium

0.2 %

Show Supplier Material materials with Calcium of 0.2 %

CaO

Iron

0.15 %

Show Supplier Material materials with Iron of 0.15 %

Fe₂O₃

Magnesium

9.4 %

Show Supplier Material materials with Magnesium of 9.4 %

MgO

Silicon

0.1 %

Show Supplier Material materials with Silicon of 0.1 %

SiO₂

Sodium

0.12 %

Show Supplier Material materials with Sodium of 0.12 %

Na₂O

Technological properties

Property
Application areas

GNPGraystar’s Sintered MAS is used in the production of refractory materials used for the sinter and transit zones of rotary furnaces in the cement industry, for the arches of electric arc furnaces, for the refractory lining of highfrequency furnaces, and various kinds of torpedo ladles and other ladles used in the steel industry.

Other

Available sizing:

Meshmm
3/63-6
6/141-3
14/280.6-1
-140-1
-280-0.06
-1700-0.090
-3250-0.045
-6350-0.020