GNPGraystar’s Fused Yttrium Oxide is a new product developed with special technology using yttrium raw material. It has the following characteristics: high purity, large crystal size, high temperature resistance, good thermal conductivity, and strong impermeability.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

True particle density

5.05 g/cm³

Show Supplier Material materials with True particle density of 5.05 g/cm³

Thermal

PropertyValue

Melting point

2410.0 °C

Show Supplier Material materials with Melting point of 2410.0 °C

Chemical properties

PropertyValueComment

Aluminium

0.01

Show Supplier Material materials with Aluminium of 0.01

max. Al₂O₃

Iron

0.01

Show Supplier Material materials with Iron of 0.01

max. Fe₂O₃

Silicon

0.02

Show Supplier Material materials with Silicon of 0.02

max. SiO₂

Titanium

0.01

Show Supplier Material materials with Titanium of 0.01

max. TiO₂

Yttrium

99.5 %

Show Supplier Material materials with Yttrium of 99.5 %

min. Y₂O₃

Technological properties

Property
Application areas

GNPGraystar’s Fused Yttrium Oxide is typically used in the titanium casting and specialty ceramics industries.

Other

Available Sizing:

  • Sizes available per customer’s requirement.