Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Synthetic Diamond Powder
GNPGraystar offers Synthetic Diamond Powder. Synthetic Diamond is characterized with some superior properties such as extreme hardness, excellent thermal conductivity, and a good chemical stability. Diamond is becoming the most popular material for abrasives, in cutting and polishing tools, and in heat sinks.
This material data has been provided by GNPGraystar Specialty Materials.
All categories
General
Property | Value | Comment |
---|---|---|
Particle size range | 54.0 µm Show Supplier Material materials with Particle size range of 54.0 µm | different specifications, please refer to the table below |
Technological properties
Property | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Application areas | GNPGraystar’s Synthetic Diamond Powder is used primarily for fine grinding, lapping, polishing tools, and polycystalline composite materials. | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Other |
Other sizes/non-powder sizes may be available - please contact us with your required sizing. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2022 Matmatch GmbH, All rights reserved.
Made with ❤️ in Munich!