Alumina Grinding Media

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Alumina Grinding Media (spherical) is high grade milling media produced by isostatic pressing and fired at high temperature. These feature high hardness, high density, low wear loss, good normalization, and good corrosion resistance

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

3.6 g/cm³

Show Supplier Material materials with Density of 3.6 g/cm³

min.

Water absorption

0.01 %

Show Supplier Material materials with Water absorption of 0.01 %

max.

Mechanical

PropertyValue

Hardness, Mohs

9.0 [-]

Show Supplier Material materials with Hardness, Mohs of 9.0 [-]

Technological properties

Property
Application areas

GNPGraystar’s Alumin Grinding Media is used in wet grinding (batch and continuous ball mills), ceramic glaze grinding, and in dry grinding of resins, ceramic raw materials, and other mineral products.

Other

Beads/Balls are available in 1, 3, 6, 8, 10, 13, 15, 18, 20, 25, 30, 35, 40, 45, 50, 60, 70, & 80 mm diamters.

Cylinders are available in 12x12, 20x20, 30x30, 35x35, 40x45, and 50x55 mm.

Other sizes/shapes available upon request.

Wear resistance

Wear rate of maximum 0.15%