Brown Aluminum Oxide Microgrits

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Brown Aluminum Oxide is fused in an electric arc furnace and produces a high strength, tough, and extremely durable grain. GNPGraystar’s brown aluminum oxide is a medium to high density product which is available in standard grades or can be custom graded for your application.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

True particle density

3.95 g/cm³

Show Supplier Material materials with True particle density of 3.95 g/cm³

Mechanical

PropertyValueComment

Hardness, Knoop, HK2

2050 [-]

Show Supplier Material materials with Hardness, Knoop, HK2 of 2050 [-]

Knoop (100)

Hardness, Mohs

9.0 [-]

Show Supplier Material materials with Hardness, Mohs of 9.0 [-]

Thermal

PropertyValue

Melting point

2000.0 °C

Show Supplier Material materials with Melting point of 2000.0 °C

Chemical properties

PropertyValueComment

Aluminium

95.62 %

Show Supplier Material materials with Aluminium of 95.62 %

Al₂O₃

Iron

0.42 %

Show Supplier Material materials with Iron of 0.42 %

Fe₂O₃

Other

0.3

Show Supplier Material materials with Other of 0.3

Silicon

1.12 %

Show Supplier Material materials with Silicon of 1.12 %

SiO₂

Titanium

2.54

Show Supplier Material materials with Titanium of 2.54

TiO₂

Technological properties

Property
Application areas

GNPGraystar’s Brown Aluminum Oxide Macrogrits are used in all types of bonded and coated abrasive applications for ferrous and normal alloy steels. It is also used in a myriad of refractory and general industrial applications.


GNPGraystar’s Brown Aluminum Oxide Microgrits are used for precision lapping, micro-blasting, fine grit bonded and coated abrasives applications, thermal coatings, and polishing compounds.

Certifications

ANSI and FEPA

Agency & Mil-Specs (such as A-A-59316 & MIL-A-22262B)

Pratt & Whitney, Rolls Royce, Praxair, Stryker, etc.

Color

Brown

Crystal structure

Alpha - Alumina

Other

Test Methods
Microgrit Sizing:FEPA F Standard 42-2:2006
FEPA P Standard 43-2:2006
JIS R 6001-1987
Custom Sizes Available