White Aluminum Oxide Macrogrits

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s White Aluminum Oxide is electrically fused in an arc furnce using Bayer process high purity alumina. The final product is used in applications where higher purity levels and lower iron content is desired as compared to brown aluminum oxide

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

True particle density

3.95 g/cm³

Show Supplier Material materials with True particle density of 3.95 g/cm³

Mechanical

PropertyValue

Hardness, Mohs

9.0 [-]

Show Supplier Material materials with Hardness, Mohs of 9.0 [-]

Thermal

PropertyValue

Melting point

2000.0 °C

Show Supplier Material materials with Melting point of 2000.0 °C

Chemical properties

PropertyValueComment

Aluminium

99.78 %

Show Supplier Material materials with Aluminium of 99.78 %

Al₂O₃

Iron

0.04 %

Show Supplier Material materials with Iron of 0.04 %

Fe₂O₃

Silicon

0.02 %

Show Supplier Material materials with Silicon of 0.02 %

SiO₂

Sodium

0.16 %

Show Supplier Material materials with Sodium of 0.16 %

Na₂O

Technological properties

Property
Application areas

GNPGraystar’s White Aluminum Oxide macrogrits are used in surface grinding, external and internal cylindrical grinding, creep-feed grinding of low or unalloyed steel. General industrial applications include pressure blasting, microderm abrasion, lapping, anti-skid, and refractories.


GNPGraystar’s White Aluminum Oxide microgrits are used for precision lapping, micro blasting, fine grit bond and coated applications, thermal coatings, polishing compounds, and more.

Certifications

ANSI and FEPA (Macrogrits); FEPA and JIS (Microgrits)

Agency & Mil-Specs

Color

White

Crystal structure

Alpha - Alumina

Other

Test Methods
Macrogrit Sizing:ANSI B74.12 Table 2
Customer Specific Standards