Black Aluminum Oxide General

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Black Aluminum Oxide is produced by fusing bauxite, iron oxide, and other elements in an arc-furnace. The resulting product has a moderate hardness, high toughness, high temperature resistance, good thermal stability, and excellent self-sharpening.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

True particle density

3.5 g/cm³

Show Supplier Material materials with True particle density of 3.5 g/cm³

Mechanical

PropertyValueComment

Hardness, Knoop, HK2

2000 [-]

Show Supplier Material materials with Hardness, Knoop, HK2 of 2000 [-]

Knoop (100)

2200 [-]

Show Supplier Material materials with Hardness, Knoop, HK2 of 2200 [-]

Knoop (100)

Hardness, Mohs

8.0 - 9.0 [-]

Show Supplier Material materials with Hardness, Mohs of 8.0 - 9.0 [-]

Thermal

PropertyValue

Melting point

2050.0 °C

Show Supplier Material materials with Melting point of 2050.0 °C

Chemical properties

PropertyValueComment

Aluminium

62 %

Show Supplier Material materials with Aluminium of 62 %

min. Al₂O₃

Iron

6.0 - 12.0 %

Show Supplier Material materials with Iron of 6.0 - 12.0 %

Fe₂O₃

Silicon

25

Show Supplier Material materials with Silicon of 25

max. SiO₂

Titanium

2.0 - 4.0 %

Show Supplier Material materials with Titanium of 2.0 - 4.0 %

TiO₂

Technological properties

Property
Application areas

GNPGraystar’s Black Aluminum Oxide, due to its thermal stability and low heat generation when polishing, is used to polish metal pieces, especially stainless steel, producing a high smooth finish with little surface discoloration. It is also used in resin bonded abrasives, blasting applications, as anti-skid surfacing material, abrasive belts, flap wheels, fiber wheels, and other polishing & lapping applications.

Color

Black

Crystal structure

Trigonal System

Other

General Black Aluminum Oxide Sizing:

3-5 mm, 1-3 mm, 0.4-1.0 mm, 0-1 mm

F12-F400 Grit (FEPA F: 42-2:2006)

Other Sizes are Available Upon Request