Description

GNPGraystar’s Precision Calcined Alumina is aluminum oxide (shape: Hexagonal Platelets) that has been heated at temperatures in excess of 1,050°C (1,922°F) to drive off nearly all chemically combined water. In this form, alumina has great chemical purity, extreme hardness (9 on the Mohs hardness scale, on which diamond is 10), high density, and a high melting point (slightly above 2,000°C [3,632°F]).

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size range

1.0 - 50.0 µm

Show Supplier Material materials with Particle size range of 1.0 - 50.0 µm

different specifications, please refer to the table below

True particle density

3.95 g/cm³

Show Supplier Material materials with True particle density of 3.95 g/cm³

pH Value

7.5 - 11.0 [-]

Show Supplier Material materials with pH Value of 7.5 - 11.0 [-]

Mechanical

PropertyValueComment

Hardness, Knoop, HK2

2100 [-]

Show Supplier Material materials with Hardness, Knoop, HK2 of 2100 [-]

Knoop (100)

Hardness, Mohs

9.0 [-]

Show Supplier Material materials with Hardness, Mohs of 9.0 [-]

Thermal

PropertyValue

Melting point

2000.0 °C

Show Supplier Material materials with Melting point of 2000.0 °C

Chemical properties

PropertyValueComment

Aluminium

99.59 %

Show Supplier Material materials with Aluminium of 99.59 %

Al₂O₃

Iron

0.03 %

Show Supplier Material materials with Iron of 0.03 %

Fe₂O₃

Silicon

0.03 %

Show Supplier Material materials with Silicon of 0.03 %

SiO₂

Sodium

0.35 %

Show Supplier Material materials with Sodium of 0.35 %

Na₂O

Technological properties

Property
Application areas

GNPGraystar’s Precision Calcined Alumina is used primarily for lapping and polishing of various products including precision optics, piezo electronics, precision bearings, optical glass, sime-conductor quartz, stainless steel, Gallium Arsenide, Germanium, and more.

Color

White

Crystal structure

Monocrystalline Alpha Alumina

Other

Sizing Available (in Microns):

1, 3, 5, 7, 9, 12, 15, 18, 20, 25, 30, 40, and 50