RockRidge Glass Beads

Want to keep this datasheet? Save it now in your required format

Description

RockRidge Glass Beads (Roundness ≥ 90 %) offer a wide array of sizes in order to ensure maximum performance for a variety of applications.


RockRidge Glass Beads offer many desirable characteristics. These characteristics include, but are not limited to, high transparency, stable chemical makeup, and high toughness, which allow for a recyclable and economical blasting media.

Related Standards

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Bulk density

1.4 - 1.6 g/cm³

Show Supplier Material materials with Bulk density of 1.4 - 1.6 g/cm³

Density

2.4 - 2.6 g/cm³

Show Supplier Material materials with Density of 2.4 - 2.6 g/cm³

Mechanical

PropertyValue

Hardness, Knoop, HK2

600 [-]

Show Supplier Material materials with Hardness, Knoop, HK2 of 600 [-]

Technological properties

Property
Certifications

RockRidge Glass Beads meet all Occupational Health and Safety Administration (OSHA) requirements. RockRidge Glass Beads do not contain free-silica and meet all ISO 11126-10:200 requirements.

Other

For typical sizings please refer to the pictures on the top right side of the datasheet