Graphene on PET Film (Continuous Monolayer >95%)

Want to keep this datasheet? Save it now in your required format

Description

State-of-the-art chemical vapour deposition (CVD) methods produce exceptionally high quality graphene film for use as transparent conductors and in other innovative applications.


In addition to offering standard samples, Goodfellow can assist customers with the transfer of graphene film onto their own substrate

Properties

General

Domain size

ddomain

10 - 20 μm

Substrate

PET, 188µm

Dimension

Length

l

600 mm

max

Width

w

500 mm

max

Electrical

Carrier mobility

µ

3500 cm²/Vs at 20 °C

Sheet resistivity

ρel,sheet

250 - 400 Ω/sq at 20 °C

Optical

Luminous transmittance

t

97 [-]

Technological properties

Application areas

Light flexible displays, plastic electronics, printed circuit boards, liquid crystal displays, thin film photovoltaics, e-paper, sensors and OLEDs

Processing history

Growth method: CVD

Do you need more data regarding this material?

This material data has been provided by Goodfellow.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.