Low Density Polyethylene (LDPE) from agricultural tunnels with moisture absorption of 0.07% (100°C - 1hr)

This material data has been provided by Green Minds Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Supplier Material materials with Density of 0.92 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.07 %

Show Supplier Material materials with Moisture absorption of 0.07 %

ASTM D6982, 100°C - 1hr

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

941 %

Show Supplier Material materials with Elongation of 941 %

ASTM D638

Tensile strength

23.0 °C

18.43 MPa

Show Supplier Material materials with Tensile strength of 18.43 MPa

ASTM D638

Technological properties

Property
Application areas

Electric Hoses - Film Grades

Color

Honey