Recycled MDPE in pellet form which is sourced 100% from drip tape. It is suitable for extrusion and injection process.

This material data has been provided by Green World Compounding.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.93 - 0.95 g/cm³

Show Supplier Material materials with Density of 0.93 - 0.95 g/cm³

ISO 1183

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

max., ISO 787/2

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

600 %

Show Supplier Material materials with Elongation of 600 %

min., ISO 527-2

Tensile strength

23.0 °C

19 MPa

Show Supplier Material materials with Tensile strength of 19 MPa

min., ISO 527-2

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

3 %

Show Supplier Material materials with Ash content of 3 %

max., ISO 3451-1, A

Rheological Properties

PropertyValueComment

Melt volume-flow rate

0.3 - 0.6 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 0.3 - 0.6 cm³/10min

190°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Drip tape, irrigation pipes, corrugated tubing, injection moulding, etc.

Color