The material: 'Low Density Polyethylene (LD PE) for Film Applications' you were looking for has been superseded by the one below.

ALFATEN 200

Want to keep this datasheet? Save it now in your required format

Description

Recycled LDPE in pellet form which is sourced from LDPE ex-greenhouse natural covering film. It is suitable for extrusion and injection process.

This material data has been provided by Green World Compounding.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Density

0.9 - 0.92 g/cm³

Show Supplier Material materials with Density of 0.9 - 0.92 g/cm³ at 23.0 °C

23.0 °C

ISO 1183

Water absorption

0.1 %

Show Supplier Material materials with Water absorption of 0.1 % at 23.0 °C

23.0 °C

max., ISO 787/2

Mechanical

PropertyValueTemperatureComment

Elongation

350 %

Show Supplier Material materials with Elongation of 350 % at 23.0 °C

23.0 °C

min., ISO 527-2

Tensile strength

10 MPa

Show Supplier Material materials with Tensile strength of 10 MPa at 23.0 °C

23.0 °C

min., ISO 527-2

Thermal

PropertyValueTemperatureComment

Ash content

3 %

Show Supplier Material materials with Ash content of 3 % at 23.0 °C

23.0 °C

max., ISO 3451-1, A

Rheological Properties

PropertyValueComment

Melt volume-flow rate

0.3 - 0.6 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 0.3 - 0.6 cm³/10min

190°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Construction, industrial & silage films, bags, hoods & sacks, injection moulding, irrigation pipes, corrugated tubing, etc.

Color

Natural