Recycled LDPE which is sourced 100% from agricultural LDPE film and characterised by enhanced filtering and fluidity and double extrusion. It is suitable for extrusion, blow molding and injection process.

This material data has been provided by Green World Compounding.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 - 0.92 g/cm³

Show Supplier Material materials with Density of 0.9 - 0.92 g/cm³

ISO 1183

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

max., ISO 787/2

Rheological Properties

PropertyValueComment

Melt volume-flow rate

0.4 - 0.8 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 0.4 - 0.8 cm³/10min

190°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Construction, industrial & silage films, bags, hoods & sacks, injection moulding, irrigation pipes, corrugated tubing, etc.

Color

Natural