ALFAFIL® 220TH

Want to keep this datasheet? Save it now in your required format

Description

Recycled PP reinforced with 20% Ultrafine Talc that has good dispersion, good mechanical properties and dimensional stability. Suitable for injection moulding.

This material data has been provided by Green World Compounding.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.02 - 1.06 g/cm³

Show Supplier Material materials with Density of 1.02 - 1.06 g/cm³

ISO 1183-1, A

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.35 - 1.65 GPa

Show Supplier Material materials with Flexural modulus of 1.35 - 1.65 GPa

ISO 178

Impact strength, Charpy unnotched

23.0 °C

30 - 40 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 30 - 40 kJ/m²

ISO 179

Rheological Properties

PropertyValueComment

Melt mass-flow rate

9 - 14 g/10min

Show Supplier Material materials with Melt mass-flow rate of 9 - 14 g/10min

230°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Injection Moulding

Color

Black, Natural

Fillers