Recycled PP reinforced with 20% Ultrafine Talc that has good dispersion, good mechanical properties and dimensional stability. Suitable for injection moulding.

This material data has been provided by Green World Compounding.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.02 - 1.06 g/cm³

Show Supplier Material materials with Density of 1.02 - 1.06 g/cm³

ISO 1183-1, A

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.35 - 1.65 GPa

Show Supplier Material materials with Flexural modulus of 1.35 - 1.65 GPa

ISO 178

Impact strength, Charpy unnotched

23.0 °C

30 - 40 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 30 - 40 kJ/m²

ISO 179

Rheological Properties

PropertyValueComment

Melt mass-flow rate

3 - 6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 3 - 6 g/10min

230°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Injection Moulding

Color

Black

Fillers

17-23% Ultrafine Talc