ALFATEN 140

Want to keep this datasheet? Save it now in your required format

Description

Recycled HDPE in pellet form which is sourced from irrigation pipe, corrugated pìpe, bottle, canister & drum. Suitable for extrusion and blow molding.

This material data has been provided by Green World Compounding.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.94 - 0.96 g/cm³

Show Supplier Material materials with Density of 0.94 - 0.96 g/cm³

ISO 1183

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

max., ISO 787/2

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

3 %

Show Supplier Material materials with Ash content of 3 %

max., ISO 3451-1, A

Rheological Properties

PropertyValueComment

Melt volume-flow rate

0.2 - 0.4 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 0.2 - 0.4 cm³/10min

190°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Films and sheets (industrial, construction, ...)

Bags and sacks

Irrigation pipe, corrugated, wiring, multilayer

Injection applications

Asphalt sheet.

Agricultural utensils, etc.

Color

Black