Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 - 0.965 g/cm³

Show Supplier Material materials with Density of 0.95 - 0.965 g/cm³

ISO 1183

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

max., ISO 787/2

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

3 %

Show Supplier Material materials with Ash content of 3 %

max., ISO 3451-1, A

Rheological Properties

PropertyValueComment

Melt mass-flow rate

4 - 8 g/10min

Show Supplier Material materials with Melt mass-flow rate of 4 - 8 g/10min

230°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Films and sheets (industrial, construction, ...)

Bags and sacks

Irrigation pipe, corrugated, wiring, multilayer

Injection applications

Asphalt sheet.

Agricultural utensils, etc.

Color