General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.95 - 0.97 g/cm³ Show Supplier Material materials with Density of 0.95 - 0.97 g/cm³ at 23.0 °C | 23.0 °C | ISO 1183 |
Water absorption | 0.1 % Show Supplier Material materials with Water absorption of 0.1 % at 23.0 °C | 23.0 °C | max., ISO 787/2 |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Ash content | 3 % Show Supplier Material materials with Ash content of 3 % at 23.0 °C | 23.0 °C | max., ISO 3451-1, A |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 4 - 8 g/10min Show Supplier Material materials with Melt mass-flow rate of 4 - 8 g/10min | 230°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Films and sheets (industrial, construction, ...) Bags and sacks Irrigation pipe, corrugated, wiring, multilayer Injection applications Asphalt sheet. Agricultural utensils, etc. | |
Color | Black, White, Green, Blue,... |