Description

Nickel with highest degree of purity with the following features:


  • Very low levels of carbon (20 ppm) and sulfur (2 ppm) which tend to segregate at grain boundries resulting in hot shortening
  • Cleanliness, absence of non-metallic inclusions as Al, Ti or Si oxides
  • Low electrical resistivity at 20°C
  • High thermal conductivity at 20°C
  • Excellent formability
  • Low softening temperature (350°C)
  • Low recrystallization temperature (350°C)
  • Improved oxidation resistance: development of tightly adherent one-layer oxide scale instead of a two-layer costumary one, which tends to flake off due to mismatch in thermal expansion.
  • Equivalent Materials

    This material data has been provided by Hpulcas GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Dimension

    PropertyValue

    Dimensions

    Plate: width: up to 625 mm, Thickness: 1-10 mm - Strip/Band: Width: 2-600 mm, Thickness: 0.1-6 mm - Foil: Width: 2-360, Thickness: 0.004-0.1 mm ; various dimensions can be also customized

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    196 GPa

    Show Supplier Material materials with Elastic modulus of 196 GPa

    Elongation

    23.0 °C

    45 %

    Show Supplier Material materials with Elongation of 45 %

    min.

    Hardness, Vickers

    23.0 °C

    65 [-]

    Show Supplier Material materials with Hardness, Vickers of 65 [-]

    max.

    Tensile strength

    23.0 °C

    300 - 350 MPa

    Show Supplier Material materials with Tensile strength of 300 - 350 MPa

    Yield strength Rp0.2

    23.0 °C

    100 - 200 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 100 - 200 MPa

    Thermal

    PropertyTemperatureValue

    Recrystallization temperature

    350 °C

    Show Supplier Material materials with Recrystallization temperature of 350 °C

    Thermal conductivity

    23.0 °C

    90.9 - 91 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 90.9 - 91 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    23.0 °C

    7.1E-8 Ω·m

    Show Supplier Material materials with Electrical resistivity of 7.1E-8 Ω·m

    Chemical properties

    PropertyValue

    Carbon

    2E-3 %

    Show Supplier Material materials with Carbon of 2E-3 %

    Nickel

    99.98 %

    Show Supplier Material materials with Nickel of 99.98 %

    Sulfur

    2E-4 %

    Show Supplier Material materials with Sulfur of 2E-4 %

    Technological properties

    Property
    Application areas

    Plate material: sputter target, gaskets with various form and dimensions, gaskets in chemical plants, gaskets in refineries, Expanded metal, construction elements in chlor-alkali electrolysis, glass forming molds, Nickel anodes for electroplating/galvanic coating/galvanic process - Strip/Coile: Pre-material for roll bonding, in batteries as current collectors and terminals; in Microbatteries as current collectors and terminals, in capacitors, micro-capacitors, supercapacitors as electrode substrate, as tapes; Nickel anodes for electroplating/galvanic coating/galvanic process, Brazing metal, pre-material to produce composites/layered braze , interlayer diffusion barrier - Foil: in batteries as current collectors and terminals, in Microbatteries as current collectors and terminals, in capacitors, micro-capacitors, multi layer ceramic capacitors, Barium Titanate multi layer ceramic capacitors, in supercapacitors as electrode substrate, as tapes, substrate in pizoelectric applications, substrate for PZT in ferroelectric memories, micromotors, microsensors and actuators, substrate in the synthesis of carbon nanotubes and graphene, substrate in the synthesis of metal oxide thin layer, , sensors, temperature sensors, gas sensors, Brazing metal, pre-material to produce composites/layered braze, interlayer diffusion barrier -, Expanded Ni Foil for Electrochemstry and fuel cells

    Heat Treatment

    Soft Annealed

    Processing history

    Hpulcas has developed a process to manufacture high purity nickel plate, strip, band, wire and flatwire directly from full plate cathodes, avoiding melt metallurgy and powder technology. Cathode plates are produced by an electro-winning process resulting in fully dense nickel plates with a minimum of trace elements. This method achieves an initial purity of 99.98% nickel. The cathode plates are hot rolled from 12 to 15 mm down to about 6 mm in one pass. After cooling, the hot rolled sheets are leveled and the oxidized surface is removed by brushing. The sheets are then cut to a rectangle of constant width by a table shear. For the production of strip and Band, the sheets are beveled, frontally welded with a high purity nickel feed wire and coiled. The hot rolled coil is then cold rolled to the desired dimensions and mechanical properties through cold rolling and intirm annealing.

    Surface Finish

    For Strip/ Band /Foil: mill finish, mirror finish, brush finish