The material: 'STOL® 76M R620S' you were looking for has been superseded by the one below.

STOL® 76M R620S

View suppliers (4)
Want to keep this datasheet? Save it now in your required format

Description

STOL® 76M is an optimized CuNiSi alloy that can be hardened by cold forming and by precipitation of NiSi-phases during a heat treatment. It has excellent bendability, excellent hot and cold forming properties, a high strength and a good corrosion resistance. Due to the NiSi-precipitations the relaxation properties, even at temperatures up to 150°C are excellent. In combination with a tin coating even at temperatures around 150°C (3.000h) the tin coating does not peel off.

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Bendability 180°, bw

23.0 °C

3 [-]

Show Material materials with Bendability 180°, bw of 3 [-]

r = x t, t <0.5mm

Bendability 180°, gw

23.0 °C

5 [-]

Show Material materials with Bendability 180°, gw of 5 [-]

r = x t, t <0.5mm

Bendability 90°, bw

23.0 °C

1.5 [-]

Show Material materials with Bendability 90°, bw of 1.5 [-]

r = x t, t <0.5mm

Bendability 90°, gw

23.0 °C

1 [-]

Show Material materials with Bendability 90°, gw of 1 [-]

r = x t, t <0.5mm

Elastic modulus

23.0 °C

118 - 135 GPa

Show Material materials with Elastic modulus of 118 - 135 GPa

depending on the condition

Elongation A50

23.0 °C

7 %

Show Material materials with Elongation A50 of 7 %

Hardness, Vickers

23.0 °C

180 - 210 [-]

Show Material materials with Hardness, Vickers of 180 - 210 [-]

Tensile strength

23.0 °C

620 - 700 MPa

Show Material materials with Tensile strength of 620 - 700 MPa

Yield strength Rp0.2

23.0 °C

560 MPa

Show Material materials with Yield strength Rp0.2 of 560 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

300.0 °C

1.68E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.68E-5 1/K

for 20°C to the mentioned temperature

Specific heat capacity

23.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Thermal conductivity

23.0 °C

260 W/(m·K)

Show Material materials with Thermal conductivity of 260 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

2.80E+7 - 3.60E+7 S/m

Show Material materials with Electrical conductivity of 2.80E+7 - 3.60E+7 S/m

Specific Electrical conductivity

57 % IACS

Show Material materials with Specific Electrical conductivity of 57 % IACS

Chemical properties

PropertyValue

Copper

Balance

Nickel

1.4 - 1.7 %

Show Material materials with Nickel of 1.4 - 1.7 %

Other

0 - 0.5 %

Show Material materials with Other of 0 - 0.5 %

Silicon

0.2 - 0.35 %

Show Material materials with Silicon of 0.2 - 0.35 %

Tin

0.02 - 0.3 %

Show Material materials with Tin of 0.02 - 0.3 %

Zinc

0.35 - 0.5 %

Show Material materials with Zinc of 0.35 - 0.5 %

Technological properties

Property
Application areas

Automotive: Switches and Relays, Contacts, Connectors, Terminals, Press fits. Electrical: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Components for the electrical industry, Stamped parts, Semiconductor Components.

Brazing

Excellent

Cold Forming

Excellent

Corrosion properties

STOL® 76M has good corrosion resistance, The alloy is insensitive to stress corrosion cracking

Heat Treatment

Temper: R620S

Hot forming

at 750-950°C, excellent

Machining

Rating 20, less suitable

Other

This alloy is in accordance with RoHS 2002/96/CE for electric & electronic equipments and 2002/53/CE for automotive industry.

Plating

Electroplating is excellent

Welding

Gas Shielded Arc Welding: Excellent, Laser Welding: Fair

Looking for suppliers of this material? Click to see 4 supplier of STOL® 76M R620S on Matmatch