CA104 - CuAl10Ni5Fe4

Alternative and trade names
CA1; CA2; X232; X87
Want to keep this datasheet? Save it now in your required format

Description

Suitable mechanical properties, sea-water and saline mist corrosion resistant, oxidation resistant.

Related Standards

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.6 g/cm³

Show Supplier Material materials with Density of 7.6 g/cm³

Dimension

PropertyValue

Dimensions

Available size round products (mm): from 16

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

125 GPa

Show Supplier Material materials with Elastic modulus of 125 GPa

Elongation

23.0 °C

12 - 15 %

Show Supplier Material materials with Elongation of 12 - 15 %

Hardness, Brinell

23.0 °C

190 [-]

Show Supplier Material materials with Hardness, Brinell of 190 [-]

Hardness, Rockwell C

23.0 °C

12 [-]

Show Supplier Material materials with Hardness, Rockwell C of 12 [-]

Hardness, Vickers

23.0 °C

186 [-]

Show Supplier Material materials with Hardness, Vickers of 186 [-]

Tensile strength

23.0 °C

650 - 700 MPa

Show Supplier Material materials with Tensile strength of 650 - 700 MPa

Yield strength

23.0 °C

320 - 400 MPa

Show Supplier Material materials with Yield strength of 320 - 400 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

40 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 40 W/(m·K)

for 20-200°C

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 5.00E+6 S/m

Magnetic

PropertyTemperatureValue

Relative magnetic permeability

23.0 °C

1.5 [-]

Show Supplier Material materials with Relative magnetic permeability of 1.5 [-]

Technological properties

Property
Application areas

Summary of typical applications: Aerospace industry: rings, bushings and bearings for landing gears; Marine industry: distributor bodies, screws, forged parts

Corrosion properties

Corrosion resistance rating: 4 out of 5

Friction

Friction behavior rating: 4 out of 5

General machinability

Machinability: 40 %