Description

Very high mechanical properties, very good resistance to sea-water corrosion and to oxidation, good impact and fatigue resistance, no sparks on impact, strictly amagnetic.

Related Standards

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.6 g/cm³

Show Supplier Material materials with Density of 8.6 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

145 GPa

Show Supplier Material materials with Elastic modulus of 145 GPa

Elongation

23.0 °C

10 %

Show Supplier Material materials with Elongation of 10 %

Hardness, Brinell

23.0 °C

225 [-]

Show Supplier Material materials with Hardness, Brinell of 225 [-]

Hardness, Rockwell C

23.0 °C

20 [-]

Show Supplier Material materials with Hardness, Rockwell C of 20 [-]

Hardness, Vickers

23.0 °C

227 [-]

Show Supplier Material materials with Hardness, Vickers of 227 [-]

Tensile strength

23.0 °C

780 - 830 MPa

Show Supplier Material materials with Tensile strength of 780 - 830 MPa

Yield strength

23.0 °C

590 - 690 MPa

Show Supplier Material materials with Yield strength of 590 - 690 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

30 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 30 W/(m·K)

for 20-200°C

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 5.00E+6 S/m

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1.01 [-]

Show Supplier Material materials with Relative magnetic permeability of 1.01 [-]

max

Technological properties

Property
Application areas

Summary of typical applications: Parts for marine industry, aerospace industry and electrical industry

Corrosion properties

Corrosion resistance rating: 5 out of 5

Friction

Friction behavior rating: 3 out of 5

General machinability

Machinability: 30 %