Niclafor® 1000 TD4 - (Rods, Wires) - CuNi9Sn6 - C72700

Want to keep this datasheet? Save it now in your required format

Description

Niclafor® 1000 is a range of Copper-Nickel-Tin (CuNi9Sn6) alloys designed and produced by Lebronze alloys (ex. CLAL). Mechanical advantages: Niclafor® 1000 exhibits very high mechanical properties, such as Tensile Strength and Yield Strength above 1,000 MPa (145 ksi) depending on temper, even at high temperatures. It has an excellent fatigue resistance and low friction, making it suitable for heavy duty applications.

High physical properties: Niclafor® exhibits high conductivity, very good corrosion resistance, magnetic properties and shielding effectiveness. A recyclable and environment-friendly solution: Niclafor® materials are beryllium-free, lead-free and cadmium-free, and are compliant with REACH and RoHs regulations.

Related Standards

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Supplier Material materials with Density of 8.9 g/cm³

Dimension

PropertyValue

Dimensions

Available size round products (mm): up to 12

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

120 GPa

Show Supplier Material materials with Elastic modulus of 120 GPa

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

Hardness, Brinell

23.0 °C

230 [-]

Show Supplier Material materials with Hardness, Brinell of 230 [-]

Hardness, Rockwell C

23.0 °C

22 [-]

Show Supplier Material materials with Hardness, Rockwell C of 22 [-]

Hardness, Vickers

23.0 °C

235 [-]

Show Supplier Material materials with Hardness, Vickers of 235 [-]

Tensile strength

23.0 °C

780 - 880 MPa

Show Supplier Material materials with Tensile strength of 780 - 880 MPa

Yield strength

23.0 °C

700 MPa

Show Supplier Material materials with Yield strength of 700 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.62E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

52 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 52 W/(m·K)

for 20-200°C

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

8.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 8.00E+6 S/m

Magnetic

PropertyTemperatureValue

Relative magnetic permeability

23.0 °C

1.01 [-]

Show Supplier Material materials with Relative magnetic permeability of 1.01 [-]

Technological properties

Property
Application areas

Niclafor can be a substitute to Copper-Titanium and Copper-Beryllium for some applications. It used in the automotive industry, for example on bushings and bearings, eg. small end rings in high performance car engines. Niclafor® is also a material of reference in the eyewear industry: its high elasticity and formability allow light and durable designs. Niclafor® is extensively used in the electronics industry, including aerospace systems, for applications such as EMI shielding and connector parts. Summary of typical applications: Electronics (Relays, EMI Shielding, etc.), Connectors, Electrical engineering, Automotive, Telecom and Mobile phones, Eyewear and Spectacles industry, Domestic appliance.

Corrosion properties

Corrosion resistance rating: 4 out of 5

General machinability

Machinability: 45 %

Processing history

Condition: TD4