Si45Z - CuSi3Fe2Zn3 - C65620

Alternative and trade names
X226
Want to keep this datasheet? Save it now in your required format

Description

Good anti-friction properties, suitable for cold forming, suitable for welding, suitable for hard and soft brazing.

Related Standards

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.6 g/cm³

Show Supplier Material materials with Density of 8.6 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

110 GPa

Show Supplier Material materials with Elastic modulus of 110 GPa

Elongation

23.0 °C

12 %

Show Supplier Material materials with Elongation of 12 %

Hardness, Brinell

23.0 °C

150 [-]

Show Supplier Material materials with Hardness, Brinell of 150 [-]

Hardness, Rockwell C

23.0 °C

0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 0 [-]

Hardness, Vickers

23.0 °C

149 [-]

Show Supplier Material materials with Hardness, Vickers of 149 [-]

Tensile strength

23.0 °C

540 MPa

Show Supplier Material materials with Tensile strength of 540 MPa

Yield strength

23.0 °C

340 MPa

Show Supplier Material materials with Yield strength of 340 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.75E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

30 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 30 W/(m·K)

for 20-200°C

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 5.00E+6 S/m

Technological properties

Property
Application areas

Summary of typical applications: Bearing cages, rotor bars for engines, valve guides

Corrosion properties

Corrosion resistance rating: 3 out of 5

Friction

Friction behavior rating: 5 out of 5

General machinability

Machinability: 30 %

Processing history

Condition: H